Properties | Unit | CAROZiiR® S | CAROZiiR® T | CAROZiiR® ST | CAROZiiR® T+ |
---|---|---|---|---|---|
Bulk Density | g/cm3 | 6.090-6.095 | 6.085-6.095 | 6.085-6.095 | 6.085-6.095 |
Chemical Composition: ZrO2 + HfO2 + Y2O3 ZrO2 Y2O3 HfO2 Al2O3 Other Oxides |
Percent Mass Fraction |
>99.5 91.6 5 3 < 0.3 < 0. |
>99.5 91.6 5 3 < 0.15 < 0.2 |
>99.5 91.6 5 3 < 0.15 < 0.2 |
>99.5 91.6 5 3 < 0.15 < 0.2 |
Microstructure: | gm | 0.25±0.05 | 0.25±0.05 | 0.25±0.05 | 0.25±0.05 |
Flexure Strength | Mpa | 1,500±100 | 13,00±100 | 800±100 | 1,200±100 |
Radioactivity | Bq/g | 0.1 | 0.08 | 0.08 | 0.05 |
Final Sintered Hardness |
HV10 | 1,450-1,500 | 1,200-1,300 | 1,100-1,200 | 1,300-1,400 |
Pre-Sintered Discs Hardness |
HV10 | 65-80 | 60-70 | 60-70 | 75-85 |
Translucency | 1-CR% (1 mm) | >40 | >43 | >49 | >47 |